Little up date. I went and picked up some parts from Blowsion. I got this and my cold fusion internal fuel fill, worx intake grate and new hood seal. I got most the pull bracket area and fuel fill area sanded.
Question, would puting two layers of 1208 over the old fuel filler hole be enough or...
Newb question that I could quite find the answer two. She. Doing two layers of 1208 bixial glass do I need to let the first layer dry first then sand or can I get the first layer on and wet and add the second?
Sent from my XT1030 using Tapatalk
So do I need to use twill? Also do I add cabosal to the epoxy when laying the fiber glass or is that just for filling areas?
Sent from my XT1030 using Tapatalk
Okay, would it be more beneficial to use Kevlar or carbon fiber? Carbon fiber is probably not sandable for a good out side finish?
Sent from my XT1030 using Tapatalk
I was talking with Blowsion and sense the SN upper hull is not glass they said to use there stuff they offer... Any input on this?
Sent from my XT1030 using Tapatalk
No offense taken, but that is what I said I was going to do. I'm going to sand/grind down the bracket mounting surface to the glass then add 2 layers or more to the surface. Also going to add a layer to the under side.
In this situation I would prefer to be told what to do so I do it right the...
The previous owner added some glass to the under side already, but I plane on sanding the top down and adding 2 layers then repainting it. The RRP bracket has a reinforcement brace and uses 6 mounting holes.
Also ordering a limiting rope along with the materials to fix the cracks from Blowsion.
I will run it as is and if I need to shorten the pole I'll just shorten the one I have. I just picked a 6/4 wetsuit and I should be able to start riding beginning of April!